Obaidi, H., Taqa, A., AL-Luazy, O. (2008). Reconditioning of Debonded Pure Titanium Bracket (Using Micro–etcher). , 8(1), 6-10. doi: 10.33899/rden.2008.9040
Hussain A Obaidi; Amer A Taqa; Omar H AL-Luazy. "Reconditioning of Debonded Pure Titanium Bracket (Using Micro–etcher)". , 8, 1, 2008, 6-10. doi: 10.33899/rden.2008.9040
Obaidi, H., Taqa, A., AL-Luazy, O. (2008). 'Reconditioning of Debonded Pure Titanium Bracket (Using Micro–etcher)', , 8(1), pp. 6-10. doi: 10.33899/rden.2008.9040
Obaidi, H., Taqa, A., AL-Luazy, O. Reconditioning of Debonded Pure Titanium Bracket (Using Micro–etcher). , 2008; 8(1): 6-10. doi: 10.33899/rden.2008.9040